Technical data of FeSiAl, FeNiMo and high flux magnetic ring

  • 2013-09-22
  • 2.21MB
  • Points it Requires : 2

77020-A7 MS-025125-8 0.250 0.110 0.110 12577021-A7 MS-025060-8 0.250 0.110 0.110 6077030-A7 MS-031125-8 0.310 0.156 0.125 12577031-A7 MS-031060-8 0.310 0.156 0.125 6077040-A7 MS-040125-8 0.400 0.200 0.156 12577041-A7 MS-040060-8 0.400 0.200 0.156 6077050-A7 MS-050125-2 0.500 0.300 0.187 12577051-A7 MS-050060-2 0.500 0.300 0.187 6077054-A7 MS-050090-2 0.500 0.300 0.187 9077055-A7 MS-050075-2 0.500 0.300 0.187 7577059-A7 MS-090060-2 0.900 0.550 79% nickel, 17% iron, and 4% molybdenumalloy powder for the lowest core losses of any powder core material.MPP cores possess many outstanding magnetic characteristics, such as high resistivity, low hysteresis and eddy current losses, excellent inductance stability after high DC magnetization or under high DC bias conditions and minimal inductance shift up to 2000 gausses under AC conditions.MAGNETICS High Flux powder cores are distributed air gap toroidal cores made from a50% nickel - 50% iron alloy powder for the highestavailable biasing capability of any powder corematerial.

unfold

You Might Like

Uploader
jasionla
 

Recommended ContentMore

Popular Components

Just Take a LookMore

EEWorld
subscription
account

EEWorld
service
account

Automotive
development
circle

About Us Customer Service Contact Information Datasheet Sitemap LatestNews


Room 1530, 15th Floor, Building B, No.18 Zhongguancun Street, Haidian District, Beijing, Postal Code: 100190 China Telephone: 008610 8235 0740

Copyright © 2005-2024 EEWORLD.com.cn, Inc. All rights reserved 京ICP证060456号 京ICP备10001474号-1 电信业务审批[2006]字第258号函 京公网安备 11010802033920号
×