Vicat Softening Temperature
CLTE - Flow
Thermal Conductivity
Electrical
Surface Resistivity
Volume Resistivity
Dielectric Constant (100 Hz)
98.0 °C
8.0E-5 cm/cm/°C
0.17 W/m/K
Nominal Value Unit
> 1.0E+13 ohm
> 1.0E+18 ohm·cm
2.50
ISO 306/A50
ISO 11359-2
DIN 52612
Test Method
IEC 60093
IEC 60093
IEC 60250
www.ides.com
UL and the UL logo are trademarks of UL LLC © 2014. All Rights Reserved.
The information presented on this datasheet was acquired by UL Prospector from the producer of the material. UL Prospector makes substantial efforts to assure the accuracy
of this data. However, UL Prospector assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the
material supplier.
Page: 1 of 2
Styrolution PS 495N
Electrical
Dissipation Factor
100 Hz
1 MHz
Flammability
Flame Rating
Styrolution - High Impact Polystyrene
Nominal Value Unit
4.0E-4
4.0E-4
Nominal Value Unit
HB
Test Method
UL 94
Test Method
IEC 60250
Processing Information
Injection
Processing (Melt) Temp
Nominal Value Unit
180 to 260 °C
Notes
1
2
Typical properties: these are not to be construed as specifications.
Rate B (120°C/h), Loading 2 (50 N)
www.ides.com
UL and the UL logo are trademarks of UL LLC © 2014. All Rights Reserved.
The information presented on this datasheet was acquired by UL Prospector from the producer of the material. UL Prospector makes substantial efforts to assure the accuracy
of this data. However, UL Prospector assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the
material supplier.
Page: 2 of 2