EEWORLDEEWORLDEEWORLD

Part Number

Search

MLB03-331-RC

Description
Multilayer Ferrite Bead s
File Size60KB,1 Pages
ManufacturerALLIED [Allied Electronics]
Download Datasheet View All

MLB03-331-RC Overview

Multilayer Ferrite Bead s

RoHS
Multilayer Ferrite Beads
MLB03
0.039±0.004
(1.0±0.10)
0.020±0.004
(0.50±0.10)
Dimensions:
Inches
(mm)
0.020±0.004
(0.50±0.10)
0.010±0.004
(0.25±0.10)
0.016
(0.40)
0.016
(0.40)
0.018
(0.46)
Allied
Part
Number
MLB03-060-RC
MLB03-100-RC
MLB03-300-RC
MLB03-330-RC
MLB03-400-RC
MLB03-470-RC
MLB03-600-RC
MLB03-700-RC
MLB03-750-RC
MLB03-800-RC
MLB03-900-RC
MLB03-101-RC
MLB03-121-RC
MLB03-151-RC
MLB03-221-RC
MLB03-241-RC
MLB03-301-RC
MLB03-331-RC
MLB03-481-RC
Impedance (
)
@ 100 MHz
+/- 25%
6
10
30
33
40
47
60
70
75
80
90
100
120
150
220
240
300
330
480
DC
Resistance
(Ω) Max.
0.05
0.05
0.30
0.30
0.30
0.40
0.40
0.40
0.40
0.40
0.50
0.50
0.50
0.50
0.50
0.50
0.80
0.80
0.80
*Rated
Current
(mA)
500
500
300
300
300
300
300
300
300
300
300
300
300
300
300
300
300
300
300
300
100
60
Features
Surface mount EMI suppression components
Nickel barrier termination for excellent resistance to solder heat
Multi layer technology
Flow and reflow soldering
Electrical
Impedance Range:
6Ω to 1500Ω
Tolerance:
25% over entire range
Operating Range:
-55ºC ~ +125ºC
Storage Temp:
Under 25ºC at 40~60% Humidity
Rated Current:
Based on temp rise not to exceed 30ºC
Resistance to Solder Heat
Pre-Heat 150ºC, 1 minute
Solder Composition: Sn/Ag3.0/Cu0.5
Solder Temp: 260±5ºC for 10sec ±1 sec.
Minimum of 75% of Electrode covered with new solder.
Impedance within 30% of initial value.
1.00
600
MLB03-601-RC
1.50
1000
MLB03-102-RC
2.00
1500
MLB03-152-RC
*Temperature rise
T=30ºC at rated current.
All specifications subject to change without notice.
Test Equipment
(Z):
HP4291A RF Impedance/Material Analyzer
(RDC):
Chen Hwa 502BC
Physical
Packaging:
10000 per 7 inch reel.
Marking:
None
714-665-1140
ALLIED COMPONENTS INTERNATIONAL
REVISED 6/18/09
www.alliedcomponents.com
[RISC-V MCU CH32V103 Review] First Look at CH32V103
I finally received the development board today. When I unpacked it, I saw the development board and debugging tools shown in Figure 1.Figure 1 Development board and debugging tools After power-on, exc...
jennyzhaojie Domestic Chip Exchange
May was quite busy, and my hand broke.
I injured my left wrist on May 1st, and cut all ten fingers on my right hand yesterday. Now it’s difficult for me to type....
littleshrimp Talking
What methods do you generally use to recruit or find jobs? Which platform is used more often?
What methods do you generally use to recruit or find jobs? Which platform is used more often? Any pitfalls or experiences?...
shijizai Talking about work
picture
The highest level of kissing...
gaoyanmei Talking
A fire broke out at Foxconn in Shenzhen, with thick smoke billowing from the scene
On June 2, according to Sina Guangdong Weibo, a fire broke out at Foxconn in Guanlan, Longhua District, Shenzhen, Guangdong. Flames shot up into the sky, black smoke filled the air, and explosions wer...
eric_wang Talking
PCB copper plating
[align=left][align=left][b][font=Microsoft YaHei UI]What kind of rules to establish[/font][/b][/align][align=left][font=Microsoft YaHei UI]To establish rules, we must first make it clear what rules we...
btty038 PCB Design

EEWorld
subscription
account

EEWorld
service
account

Automotive
development
circle

Datasheet   0 1 2 3 4 5 6 7 8 9 A B C D E F G H I J K L M N O P Q R S T U V W X Y Z
Room 1530, 15th Floor, Building B, No. 18 Zhongguancun Street, Haidian District, Beijing Telephone: (010) 82350740 Postal Code: 100190
Copyright © 2005-2024 EEWORLD.com.cn, Inc. All rights reserved 京ICP证060456号 京ICP备10001474号-1 电信业务审批[2006]字第258号函 京公网安备 11010802033920号